설명
성형에 필요한 윤활제 등이 포함되어 있기 때문에 바로 성형을 할 수 있습니다.
사양
| Inspection Characteristic | Unit | Lower Limiting Value | Upper Limiting Value | Desired Value | Indicative Value | Method |
| Physical Physical analysis : |
||||||
| Sieve analysis ISO 4497 cumulative : > 160 ㎛ | % | 1,00 | IN.V.1007 | |||
| Sieve analysis ISO 4497 cumulative : > 45 ㎛ | % | 40,00 | 60,00 | IN.V.1007 | ||
| Sieve analysis ISO 4497 cumulative : < 45 ㎛ | % | 40,00 | 60,00 | IN.V.1007 | ||
| Apparent density ISO 3923/1 - 2,5 mm | g/cm3 | 2,90 | 3,20 | IN.V.1010 | ||
| Flowability ISO 4490 - 2,5 mm | s | 35,0 | IN.V.1004 | |||
| Chemical Chemical analysis : |
||||||
| Tin (Sn) | % | 9,50000 | 10,50000 | IN.V.1138 | ||
| Frittage Sintering : |
||||||
| Green density | N/mm2 | 6,00 | IN.V.1020 | |||
| Green strength | N/mm2 | 4,00 | IN.V.1022 | |||
| Sintering atmosphere 75% H2/25% N2 | IN.V.1150 | |||||
| Dewaxing at 450℃ | min | 20,00 | IN.V.1150 | |||
| Sintering at 760℃ | min | 15,00 | IN.V.1150 | |||
| Dimensional change | % | -1,15 | -0,85 | IN.V.1149 | ||
| Dimensional change of standard | % | -1,15 | -0,85 | IN.V.1149 | ||
| Radial crushing strength | N/mm2 | 150 | IN.V.1022 | |||
| Radial crushing strength of standard | N/mm2 | 150 | IN.V.1022 | |||